PLA+

Use it for: functional prototypes, brackets that see handling, everyday prints.

nozzle 200230°Cbed 5060°Cdrying: low

PLA+ · slicer settings

PLA+ print settings table
Nozzle temperature200230°C
Bed temperature5060°C
EnclosureNot needed
Hardened nozzleNot needed
DryingLow — usable from the box

Strengths & weaknesses

  • Strengths: PLA ease with noticeably better impact resistance and layer adhesion.
  • Weaknesses: still heat-soft like PLA; formulations vary by brand.
  • Use it for: functional prototypes, brackets that see handling, everyday prints.

Which printers print PLA+ clean?

Verdicts below come from the documented compatibility rules — bed and hotend ceilings, enclosure, and nozzle hardness — applied identically to all 9 printers in the database. 9 print it clean.

FAQ

What temperature should I print PLA+ at?

Nozzle 200–230°C, bed 50–60°C. Start mid-range and tune with a temperature tower — exact sweet spots vary by brand and color.

Does PLA+ need an enclosure?

No — PLA+ prints fine on an open-frame printer. Normal indoor conditions are all it needs; an enclosure is optional.

Does PLA+ need drying?

PLA+ is forgiving about moisture. Sensible storage (a sealed bag with desiccant) is enough — most spools print fine straight from the box.